Component:
|
PU
|
|||
Appearance:
|
Liquid
|
|||
Color:
|
Light Yellow or Brown
|
|||
Toxicity:
|
Non-toxic
|
|||
Viscidity:
|
Approx. 800-1500CPS
|
|||
Solid Content(%)
|
65%-72%
|
|||
Shear Strength(Mpa)
|
≥2
|
1、Ready the scrap foam and pu adhesive according to the ratio of 100:6. 2、Stir→put it into the mold box→press 3、Under the condition of steam heating, shaping 10 ~ 30 minutes. 4、It will take 2 ~ 4 hours to solidify in summer at room temperature generally,and will take 8~24 hours in winter.
Normally, gross weight: 200kg/barrel. it is about 16000kg (80 drums) for a 20” container.